@article { author = {Khanchi, A and Rafati, H and Rezvaniyanzadeh, M.R}, title = {Recovery of some Rare Earth Elements from Leach Liquor of the Saghand Uranium Ore Using Combined Precipitation and Cation Exchange Methods}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {1-8}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {In this research work, the recovery and separation of La(III), Ce(III), Sm(III), Dy(III) and Nd(III) from Saghand uranium ore have been studied by precipitation and ion-exchange chromatography methods using Dowex 50W-X8 cation exchanger. At first, some preliminary and preconcentration experiments such as comminution, sieve analysis, gravity table and electrostatic in preconcentration of lanthanides were performed. Then, acidic digesting and leaching procedure were used. The results of experiments showed that rare earth elements, along with interfering ions such as Al(III), Fe(III), Mg(II) and Mn(II) present in the leach liquor solution. The investigation of separation process by precipitation method revealed that precipitation and then fast separation using centrifugal technique had the best results in the elimination of interference elements. In order to separate the lanthanides and to obtain their elution curves, the chromatographic column containing Dowex 50W-X8 resin was employed. For efficient separation of lanthanides from interference elements the hydrochloric acid with concentration of two and six molar was used respectively. Recovery of lanthanides from the leach liquor solution was achieved more than 85%.}, keywords = {Rare Earths,Uranium Ores,Precipitation,Ion Exchange Chromatography,Ion Exchange Resins,Saghand}, title_fa = {بازیابی برخی از عناصر خاکی کمیاب از محلول فروشویی حاصل از سنگ معدن اورانیوم ساغند با استفاده از تلفیق روش رسوب‌گیری با تبادل یونی}, abstract_fa = {در این کار پژوهشی، بازیابی و جداسازی La(III)، Ce(III)، Sm(III)، Dy(III) و Nd(III) از برخی یون‌های مزاحم موجود در محلول فروشویی مادة معدنی اورانیوم ساغند با استفاده از روش‌های رسوب‌گیری و کروماتوگرافی تبادل یونی به وسیله مبادله‌کنندة کاتیونی Dowex 50W-X8 مورد بررسی قرار گرفت. ابتدا آزمایش‌های مقدماتی و پیش تغلیظ از جمله: خردایش، تجزیه سرندی، میز ثقلی و جدایش الکتروستاتیکی بر روی نمونة معرف مادة معدنی ساغند به منظور تهیة کنسانتره صورت گرفت. سپس عملیات هضم اسیدی و در نهایت فروشویی اسیدی انجام شد. آنالیز محلول فروشویی نشان داد که علاوه بر عناصر خاکی کمیاب، یون‌های مزاحمی مانند Al(III)، Fe(III)، Mg(II) و Mn(II) نیز در محلول وجود دارند. بررسی‌ها بر روی فرایند جداسازی به وسیله رسوب‌گیری نشان داد که رسوب‌گیری سریع و بدنبال آن استفاده از روش سانتریفیوژ، نتایج خوبی در کاهش این کاتیون‌ها بدون حذف لانتانیدها از محلول دارد. همچنین آزمایش‌های دینامیکی به منظور جداسازی با ستون کروماتوگرافی مبادله‌کنندة کاتیونی Dowex 50W-X8 انجام گرفت. جداسازی عناصر مزاحم و لانتانیدها با استفاده از اسیدکلریدریک با غلظت‌های 2 و 6 مولار صورت گرفت. بازیابی لانتانیدها از محلول در این روش بیش از 85% بود.}, keywords_fa = {عناصر خاکی کمیاب,سنگ‌های معدن اورانیوم,رسوب‌گیری,کروماتوگرافی تبادل یونی,رزین‌های تبادل یونی,ساغند}, url = {https://jonsat.nstri.ir/article_537.html}, eprint = {https://jonsat.nstri.ir/article_537_b3a44a0e4243acfaff95fa5079871a35.pdf} } @article { author = {Aminfar, H and Ghafari, M.H}, title = {Analytical and Numerical Heat Transfer Analysis of Eccentric Fuel Pellets in a Fuel Element of Nuclear Reactor}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {9-18}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {A fuel element in nuclear reactors generally consists of fuel pellets, gaseous gap and cladding. Normally the pellets and cladding are coaxial. In this case; heat conduction equation in the fuel element is two dimensional, independent on angle (θ). Certainly elimination of gaseous gap in one direction (eccentricity of fuel pellets), will increase cladding and coolant temperature at the same direction. In this work, three dimensional analytical and numerical steady state heat transfer behavior in eccentric fuel element were studied to determine maximum temperature of fuel pellets, cladding, and coolant. Good agreement between analytical and numerical results was obtained. It is concluded that because of eccentricity of fuel element, melting of cladding and boiling in coolant will not occur.}, keywords = {Three Dimensional Calculations,Fuel Element,Gaseous Gap,Cladding,Fuel Pellets,Coolant,Eccentric,Comparative Evaluations}, title_fa = {آنالیز انتقال حرارت در حالت غیر هم محور بودن قرص‌های سوخت و غلاف در میله سوخت رآکتور هسته‌ای به روش‌های تحلیلی و عددی}, abstract_fa = {میله سوخت رآکتور هسته­ای متشکل ازقرص­های سوخت، فاصله گازی وغلاف می­باشد که در حالت عادی قرص­های سوخت و غلاف پیرامون آنها هم‌محور بوده و فاصله گازی هم در حدفاصل این دو جزء قرار گرفته است. در این حالت معادله انتقال حرارت در میله سوخت دو بعدی است و به زاویه بستگی ندارد. مسلماً حذف شدن فاصله گازی در یک جهت خاص (حالت غیرهم محوری قرص­های سوخت و غلاف)، منجر به افزایش دمای غلاف و سیال خنک‌کننده در آن جهت خواهد شد. در این پژوهش نحوه توزیع درجه حرارت در سه بعد برای یک میله سوخت، به دو روش تحلیلی و عددی در حالت پایا، برای بدست آوردن ماکزیموم درجه حرارت در قرص­های سوخت، غلاف و سیال خنک‌کننده مورد بررسی قرار گرفته است. نتایج حاصل از دو روش تحلیلی و عددی تطابق خوبی با هم داشته و نشان می­دهند پدیده­هایی چون ذوب موضعی غلاف و جوشش سیال بوجود نخواهند آمد.}, keywords_fa = {محاسبات سه‌بعدی,میلة سوخت,فاصله گازی,غلاف,قرص‌های سوخت,سیال خنک‌کننده,غیر هم محور,ارزیابی‌های تطبیقی}, url = {https://jonsat.nstri.ir/article_538.html}, eprint = {https://jonsat.nstri.ir/article_538_c80780b8d871b1d88153644190898895.pdf} } @article { author = {Nilchi, A and Abolhasanloo, G and Yaftian, M.R and Rasouli Garmarodi, S}, title = {Synthesize and Investigation of Hydrous Cerium Oxide Exchange Properties for 140Ba and 90Sr Cations–Determination of Distribution Coefficient for 152Eu and 134 Cs Cations}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {19-23}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {Hydrated cerium (IV) dioxide has been synthesized by adding excess cerium sulphate to 4M ammonia solution at 250C and pH=12.5 with constant stirring. The properties of the compound were investigated by means of infrared and thermogravimetric techniques. The effect of temperature and pH on the adsorption of Ba and Sr ions and also the distribution coefficients of Cs and Eu at various pH values on cerium (IV) dioxide were considered. The distribution coefficient results showed that with the increase of pH of the media, the amount of adsorption of Ba and Sr cations on the surface of cerium (IV) dioxide increases, and this is due to their amphoteric nature of this oxide.}, keywords = {Inorganic Ion Exchanger,Hydrous Oxide,Adsorption,Distribution Coefficient}, title_fa = {سنتز و بررسی خصوصیات تبادلی سریوم اکسید هیدراته برای کاتیون‌های 140Ba، 90Sr تعیین ضریب توزیع کاتیون‌های 152Eu و 134Cs}, abstract_fa = {سریوم (IV) اکسید هیدراته از افزودن تدریجی محلول سولفات سریوم اشباع شده به محلول 4 مولار آمونیاک در دمای 25 درجه سانتی‌گراد و 5/12=pH تهیه گردید. خواص ترکیب بدست آمده با استفاده از روش‌های طیف‌سنجی مادون قرمز و آنالیز ترموگراویمتری مورد مطالعه قرار گرفت. تأثیر تغییرات دما و pH در میزان جذب سطحی کاتیون‌های باریوم و استرانسیوم، همچنین ضریب توزیع کاتیون‌های سزیوم و یورپیوم بر روی اکسید سریوم هیدراته در pH های مختلف مطالعه شد. بررسی مقادیر ضرایب توزیع نشان داد که با افزایش pH محلول، میزان جذب سطحی کاتیون‌های باریوم و استرانسیوم بر روی اکسید سریوم آبدار افزایش می‌یابد که دلیل آن خصلت آمفوتری این اکسید است.}, keywords_fa = {مبادله‌کننده یونی معدنی,اکسید هیدراته,جذب سطحی,ضریب توزیع}, url = {https://jonsat.nstri.ir/article_539.html}, eprint = {https://jonsat.nstri.ir/article_539_c7d94547a6a91cb58dafd1b2907eaed8.pdf} } @article { author = {Jowzaee, S and Vahabi Moghaddam, M and Aliabadi, M and Hafezi, S and Attarilar, A and Hosseini, S}, title = {Gross Alpha and Beta Measurements of Spring Waters in Southwest Caspian Region by LSC and EPA 900 Methods}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {24-27}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {Determination of natural and man-made radionuclide inventories in water resources is of great importance. Gross α and β measurements are usually carried out as part of such studies. These paper reports measurements performed on water samples from springs in the southwest of caspian region by liquid scintillation method using Wallac-Quantulus 1220 system, 20ml polyethylene vials and Optiphase Hisafe 3 cocktail. With a counting time of 500min, the MDL for gross α and β measurements are 5.36 and 22.26 mBq l-1, respectively. Measurements by EPA 900 technique have also been applied for some samples and the results are compared.}, keywords = {Water Springs,Radioactivity,Gross Alpha,Gross Beta,Liquid Scintillation Detector EPA 900}, title_fa = {تعیین میزان پرتوزایی کل آلفا و بتای چشمه‌های آب منطقه جنوب غربی دریای خزر با دو روش شمارنده سنتیلاسیون مایع و EPA 900}, abstract_fa = {مواد پرتوزای طبیعی و مصنوعی از دسته آلاینده‌هایی هستند که در اکوسیستم‌های طبیعی از جمله منابع آبی یافت می‌شوند و تعیین وجود این دسته از مواد در آب از اهمیت ویژه‌ای برخوردار است. بررسی پرتوزایی آلفا و بتای کل از جمله سنجش‌های مطرح در نمونه‌های آب می‌باشد. به این منظور، تعدادی از چشمه‌های آب معدنی منطقه جنوب غربی دریای خزر به وسیله تکنیک جدید شمارنده سنتیلاسیون مایع با تفکیک‌کننده آلفا و بتا مورد آنالیز قرار گرفت. برای اندازه‌گیری نمونه‌ها، دستگاه شمارنده Wallac-Quantulus 1220، ویال‌هایی از جنس پلی‌اتیلن با حجم ml20 و مایع سنتیلاسیون Optiphase Hisafe 3 مورد استفاده قرار گرفت. مدت شمارش برای هر یک از نمونه‌ها 500 دقیقه تعیین شد. کمترین حد آشکارسازی در این روش برای آلفا و بتای کل به ترتیب برابر 1-mBq l 5.36  و 1-mBq l 22.26  است. همچنین برای تعدادی از نمونه‌ها، داده‌های حاصل از تکنیک جدید LSC با روش EPA 900 مقایسه شد.}, keywords_fa = {چشمه‌های آب,پرتوزایی,آلفا کل,بتا کل,آشکارساز سنتیلاسیون مایع,EPA 900}, url = {https://jonsat.nstri.ir/article_540.html}, eprint = {https://jonsat.nstri.ir/article_540_bc7c65929c6f338f2a6f82817d59b6d2.pdf} } @article { author = {Pazirandeh, A and Saghati, D}, title = {Study of Reactivity Effect on Dynamic Behavior of VVER-1000 Reactor Core}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {28-34}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {In the study of stability of VVER-1000 reactor core the state variables method and Routh criterion were used. By calculating temperature reactivity coefficients for fuel and moderator we have shown that the reactor core remains stable against 1$ reactivity or less than 1$. The coefficients were calculated for different concentration of boric acid as a function of temperature. The concentration above 1800ppm prevails itself as a positive effect. It should be noted that 1800ppm boric acid concentration had minimal effect on fuel temperature reactivity coefficient. The simulation calculation for 1$ reactivity insertion showed that the prompt neutron life time between 2 to 50µs causes sharp rise in flux for shorter lifetime, while decays remain more or less the same for 2 to 50µs prompt neutron lifetime.}, keywords = {Stability,Reactor Dynamics,Routh Criterion,VVER-1000}, title_fa = {بررسی اثر رآکتیویته بر رفتار دینامیکی قلب رآکتور VVER-1000}, abstract_fa = {در بررسی پایداری قلب رآکتور 3000 مگاواتی VVER-1000، با استفاده از متغییرهای حالت و معیار روث همراه با تعیین ضرائب دمایی رآکتیویته سوخت و کندکننده نشان داده‌ایم که قلب رآکتور در مقابل اعمال رآکتیویته یک دلار و زیر یک دلار پایدار است. ضرائب دمایی سوخت و کندکننده را برحسب غلظت اسید بوریک و دما حساب کرده‌ایم؛ نتایج حاصل نشان داد که هر چه غلظت اسید بوریک در کندکننده بیشتر باشد، به علت جابجایی طیف نوترون حرارتی، اثرهای متفاوتی بر ضریب دمایی رآکتیویته داشته و برای غلظت‌های بیش از ppm1800 اثر مثبتی بر ضریب دمایی رآکتیویته کندکننده دارد، در حالیکه تغییر غلظت اسید بوریک تأثیر زیادی بر ضریب دمایی رآکتیویته سوخت ندارد. محاسبات نشان داد که رفتار دینامیکی رآکتور برای طول عمر نوترون‌های آنی بین 2 تا 50 میکرو ثانیه، هرچه طول عمر نوترون‌های آنی کمتر باشد خیزش شار سریعتر و بیشتر است ولی روند افت شار کم و بیش یکسان است.    }, keywords_fa = {پایداری,دینامیک رآکتور,معیار روث,VVER-1000}, url = {https://jonsat.nstri.ir/article_541.html}, eprint = {https://jonsat.nstri.ir/article_541_db79031a59892af686754bd31ad045a1.pdf} } @article { author = {Abolghasemi, H and Rostamnejad, M and Momenzade, S and Hadadi, N}, title = {Application of Natural Vermiculite for Cesium Removal from Radioactive Aqueous Waste}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {35-39}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {The adsorption behavior of natural vermiculite for cesium (137Cs), in radioactive aqueous waste, has been investigated. Our experiments, aimed at the study of the effect of some parameters such as residential time (for batch equilibrium), pH, temperature, and flow rate (for column tests) on the efficiency of adsorption operation. The adsorption experiments were performed using both static batch equilibration and flow-through tests. The maximum adsorption was observed in alkaline condition (0.01 mol L-1 NaOH solution), using 1gr of adsorbent for 100ml of radioactive liquid waste at 60ºC, in 24h of residential time for a batch experiment. Finally, with the result of the column experiments, the breaktrough isotherm has been drawn. The present work deals with a series of experiments to assess the potential of vermiculite for the removal of radio cesium from radioactive aqueous waste. The results of these investigations are expected to be valuable, in order to reach at a higher degree of radioactive waste decontamination.}, keywords = {Adsorption,Radio Cesium(137Cs),Vermiculite,Radioactive Wastes}, title_fa = {بررسی عملکرد جاذب ورمیکولیت برای حذف سزیوم از پسمان مایع پرتوزا حاصل از رآکتور تحقیقاتی تهران}, abstract_fa = {در این کار پژوهشی، توان ورمیکولیت تولید شده در ایران به عنوان یک جاذب طبیعی، برای حذف سزیوم (137Cs) از پسمان‌های مایع پرتوزا حاصل از رآکتور تحقیقاتی تهران مورد بررسی و آزمایش قرار گرفته است.آزمایش‌ها در دو سیستم ناپیوسته و پیوسته انجام شده‌اند. هدف از انجام دادن آنها، بهینه‌سازی پارامترهای مؤثر بر فرایند جذب سزیوم به وسیله ورمیکولیت می‌باشد. پارامترهای مورد بررسی عبارتند از: زمان اقامت (برای آزمایشهای انجام شده در سیستم ناپیوسته)، pH محلول، دما و سرعت عبور جریان (برای سیستم ستونی). نتایج حاصل از آزمایش‌ها نشان می‌دهند که بیشترین میزان جذب سزیوم در محلول‌های بازی (0.01 mol.L-1 NaOH) در دمای ºC60 و با در نظر گرفتن 24 ساعت زمان تماس، برای 1 گرم ورمیکولیت در ml100 از پسمان مایع پرتوزا رخ می‌دهد. در پایان با توجه به داده‌های به دست آمده از آزمایش‌های پیوسته نمودار شکست این فرایند جذب رسم شده است. انتظار می‌رود که نتایج حاصل از این آزمایش‌ها در رسیدن به روشی کارآمد و ارزان برای آمایش پسمان‌های مایع پرتوزا مؤثر باشد.}, keywords_fa = {جذب سطحی,رادیوسزیوم ( 137Cs ),ورمیکولیت,پسمانده‌های پرتوزا}, url = {https://jonsat.nstri.ir/article_542.html}, eprint = {https://jonsat.nstri.ir/article_542_66eb9af9802b9c0d450e7e567ccbf804.pdf} } @article { author = {Ghadiri, A and Hajati, A and Alaghband, A.H and Asgari, R and Valivand, A}, title = {Design of Thickener for Separation of Acidic Leach Liquor from Residual Solid Particles in Bandar Abbas Uranium Plant}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {40-44}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {Solid-liquid separation is one of the most important sections in mineral processing. High percentage of clay material and fine particles (-200 mesh) cause different problems in separation of uranium leach liquor from the residual solid particles in filtration unit of Bandar Abbas Uranium Plant (BUP). The laboratory tests showed that thickener is a suitable device for solid-liquid separation, after leaching unit. For this reason, thickeners were selected for separating of leach liquor from the residual solid particles. For determination of the size and number of thickeners, sedimentation experiments were performed with different flocculants, “Magna floc LT-25” was selected as a suitable flocculant in 75 g/ton. The diameter of thickener was determined to be 13-14 m. In the counter current decantation (CCD), the loss percentage of uranium, using 5 thickeners, was selected to be 2.09%.}, keywords = {Thickener,Uranium Oxide,Magna floc LT-25,Separation Processes}, title_fa = {طراحی سیستم تیکنر برای جداسازی محلول فروشویی اسیدی از ذرات جامد در کارخانه اکسید اورانیوم بندرعباس}, abstract_fa = {فرایند جداسازی جامد از مایع، یکی از بخش‌های مهم در کارخانه‌های کانه‌آرایی و فرآوری مواد معدنی محسوب می‌شود. یکی از مشکلات موجود در کارخانه اکسید اورانیوم بندرعباس، جداسازی فاز محلول حاوی اورانیوم از مواد جامد باقیمانده پس از فروشویی است. وجود ترکیبات رس‌دار و درصد نرمه بالا (زیر 200 مش) در خوراک ورودی به واحد فروشویی، مشکلات فراوانی را در بخش تصفیه ایجاد نموده است. برای این منظور، آزمایشهایی برای بررسی فرایند جداسازی محلول از جامد انجام گردید. نتایج بررسی‌ها نشان داد که تیکنر، گزینه مناسبی برای جداسازی محلول از جامد، در فرایند پس از فروشویی کارخانه بندرعباس است. با انجام آزمایش‌های ته‌نشینی، لخته‌ساز (فلوکولانت) مناسب جهت فرایند تیکنر، Magna floc LT-25 با غلظت 75 (گرم در هر تن خاک) تعیین گردید. همچنین با انجام آزمایش‌های متعدد برای تعیین قطر تیکنر، این قطر در حدود 14-13 متر حساب شد. برای جلوگیری از اتلاف اورانیوم محلول در دوغاب حاصل از فروشویی، 5 تیکنر شستشو با جریان مخالف پیشنهاد شد. درصد اتلاف اورانیوم محلول با 5 تیکنر جریان مخالف، 2.09%  تعیین گردید.}, keywords_fa = {تیکنر,اکسید اورانیوم,Magna floc LT-25,فرایندهای جداسازی}, url = {https://jonsat.nstri.ir/article_543.html}, eprint = {https://jonsat.nstri.ir/article_543_d73888dcf7f2d7bc532769615bb65f19.pdf} } @article { author = {Siminfar, A.R and Shahidi, F and Hassanzadeh, M.R}, title = {Design and Implementation of an Optimized Network for a Computer Controlled Radiation Monitoring System}, journal = {Journal of Nuclear Science and Technology (JONSAT)}, volume = {29}, number = {2}, pages = {45-50}, year = {2008}, publisher = {Nuclear Science and Technology Research Institute}, issn = {1735-1871}, eissn = {2676-5861}, doi = {}, abstract = {A new design of hardware and software required for networking a computer controlled radiation monitoring system is presented. This radiation monitoring system comprises a network of area radiation monitors connected to a central computer via an interface module. The monitors are employed for area dose-rate measurement and controlled via the network. For increasing the distance between monitors and central control and reducing the transmission error, a kind of bus networking which is controlled by the interface module is used. The interface module is specially designed for network control and acts as an bus master. With this interface, there is no need to Ethernet cards in each dose monitor. Communication between the monitors and bus master is carried out by two transmission lines to send and receive, using RS485 standard to benefit by a low cost and simple hardware. In this communication platform, a special protocol is used to reduce the transmission error. This kind of networking is an optimum solution for distributed monitoring systems.}, keywords = {Monitoring System,Area Radiation Monitor,Data Transmission,Computer Networks,Radiometers,Ionizing Radiation}, title_fa = {طراحی و پیاده‌سازی شبکه‌ای بهینه برای سیستم مانیتورینگ پرتوهای یونساز با کنترل کامپیوتری}, abstract_fa = {در این مقاله نحوه طراحی سخت‌افزار و نرم‌افزار لازم برای شبکه‌بندی یک سیستم مانیتورینگ پرتو با کنترل کامپیوتری ارائه شده است. سیستم مانیتورینگ پرتو از تعدادی دستگاه اندازه‌گیری و ثبت پرتو یا رادیومتر محیطی تشکیل شده که به وسیله یک دستگاه واسط به کامپیوتر مرکزی متصل شده و تحت شبکه کنترل قرار می‌گیرند. در این سیستم برای افزودن فاصله محل نصب رادیومترهای محیطی با کامپیوتر مرکزی و کاستن احتمال بروز خطا، یک شبکه گذرگاهی با قابلیت زیاد طراحی و پروتکل ارتباطی مناسبی بکار گرفته شده است که در آن ارتباط رادیومترهای محیطی سیستم با دستگاه واسط که بعنوان کنترل‌کننده گذرگاه عمل می‌کند، برقرار و از طریق آن به کامپیوتر متصل می‌شوند. شبکه‌بندی رادیومترهای محیطی با کابل‌هایی از نوع CAT5، با استفاده از استاندارد RS485 انجام گرفته است که دارای سخت‌افزار ساده و کم‌هزینه می‌باشد. نتیجه اجرای این شبکه، ارائه راه ‌حل مناسب برای مانیتورینگ سیستم‌های توزیع شده است.}, keywords_fa = {سیستم مانیتورینگ,رادیومتر محیطی,انتقال داده‌ها,شبکه‌های کامپیوتری,پرتو سنج‌ها,تابش‌های یونساز}, url = {https://jonsat.nstri.ir/article_544.html}, eprint = {https://jonsat.nstri.ir/article_544_b568e556b0c2f536b09a016c157c4d06.pdf} }